1.
The synthesis conditions of belite-calcium barium sulphoaluminate cement clinker were studied by the orthogonal test method.
采用正交试验方法研究了贝利特—硫铝酸钡钙水泥熟料的煅烧条件。
2.
Synthesis conditions and mechanical performance of belite-calcium barium sulphoaluminate cement clinker were investigated by the orthogonal test taking clinker modulus and content of calcium barium sulphoaluminate(C_(2.
选择熟料率值和硫铝酸钡钙掺量为影响因素,通过正交试验研究了贝利特—硫铝酸钡钙水泥的合成条件和力学性能,并利用XRD、SEM-EDS等测试手段分析了该水泥熟料的组成和结构。
3.
Belite–calcium barium sulphoaluminate cement is a new type of cementitious material.
贝利特–硫铝酸钡钙水泥是一种新型的水泥材料,通过在贝利特熟料矿物体系中引入硫铝酸钡钙矿物,达到提高贝利特水泥早期强度的目的。
6) Ba-bearing calcium sulphoaluminate
硫铝酸钡钙
1.
The influence of calcium fluoride(CaF2),temperature and liquid phase(C4AF is selected in the paper) on the mineral formation of tri-calcium silicate(C3S) and Ba-bearing calcium sulphoaluminate(CBAS,the chemical measure is selected as 2.
以纯化学试剂配料,研究了微量元素氟化钙(CaF2)、温度以及液相(本文取铁铝酸四钙)等不同条件下对硅酸三钙(C3S)和硫铝酸钡钙(CBAS,本文取化学计量为2。
2.
A new series of Ba-bearing calcium sulphoaluminate minerals are synthesized by replacing CaSO 4 in the C 4A 3 with different amounts of BaSO 4.
硫铝酸钡钙是一种性能优良的水泥新矿物 ,以该矿物为基础生产了性能优良的含钡硫铝酸盐水泥。
补充资料:氧化钡
BaO 分子量 158.36
白色或浅灰色多孔物,易碎为粉求。有时制得得氧化钡为细小的等轴晶系结晶体。密度5.32-5.72g/cm3。熔点1923℃。极易从空气中吸收水分及二氧化碳而形成碳酸钡。与水作用生成氢氧化钡。
应用 用于精练甜莱,制备过氧化钡和钡盐,以及用作脱水剂等。近来广泛用作气体的于燥剂,其效用远远超过石灰、氯化钙和铝胶等。此外,还用于玻璃、陶瓷工业。
白色或浅灰色多孔物,易碎为粉求。有时制得得氧化钡为细小的等轴晶系结晶体。密度5.32-5.72g/cm3。熔点1923℃。极易从空气中吸收水分及二氧化碳而形成碳酸钡。与水作用生成氢氧化钡。
应用 用于精练甜莱,制备过氧化钡和钡盐,以及用作脱水剂等。近来广泛用作气体的于燥剂,其效用远远超过石灰、氯化钙和铝胶等。此外,还用于玻璃、陶瓷工业。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条