1) Activated zeolite

活化沸石
1.
The experiments inside and outside the lab indicate that activated zeolite can not only remove ironion, but also fluorine from fluorine container water.
室内外试验研究表明,活化沸石不仅有优良除铁性能,而且对氟化物也有良好的去除效果,经简单工艺处理后,可以使超标含铁含氟水达到饮用水卫生标准,是一种新型多功能净水材料。
2.
The activated zeolite was also used to adsorb ammonia-nitrogen from coal-coking wastewater pretreated by SBR-oxidation.
3mol·L-1NaCl活化后,对氨氮的吸附效果最佳;当活化沸石投加量为10g·L-1、接触时间为40min时,氨氮去除率可达88。
2) deactivated zeolite

减活化沸石
3) Na-pretreated zeolite

钠型活化沸石
1.
Study on the ammonia removal from wastewater by Na-pretreated zeolite;

钠型活化沸石去除水中氨氮的实验研究
4) Surfactant-modified zeolit

表面活化沸石
5) magnesium-actived zeolite

镁型活化沸石
1.
Study on the capacity of defluorination by magnesium-actived zeolite;

镁型活化沸石除氟性能研究
6) iron-active clinoptilolite

铁活化斜发沸石
补充资料:4A沸石
分子式:
CAS号:
性质:又称Na12[(A1O2)12、(SiO2)12]27H2O 又称4A分子筛。白色固体颗粒。呈网络状结构,内含均匀小孔,孔径0.42nm,比表面积约为600m2/R,不溶于水和有机溶剂,能溶解于强碱和强酸。加热超过800℃时,重新结晶形成白硅石状的结构。有吸附水分,液体、气体及不饱和的有机物质。对钙离子有交换能力,理论交换能力为352CaCO3mg/g,一般为290~320mgCaCO3/g,白度≥95%,pH值10~11.5,表观密度0.3~0.5g/cm3,平均粒径为2μm,粒度分布≤4μm占85%以上。用作无磷洗涤剂的助剂,代替三聚磷酸钠;在石油和其他工业用作气体和液体的干燥、脱水净化等,也用作催化剂和软水剂。
CAS号:
性质:又称Na12[(A1O2)12、(SiO2)12]27H2O 又称4A分子筛。白色固体颗粒。呈网络状结构,内含均匀小孔,孔径0.42nm,比表面积约为600m2/R,不溶于水和有机溶剂,能溶解于强碱和强酸。加热超过800℃时,重新结晶形成白硅石状的结构。有吸附水分,液体、气体及不饱和的有机物质。对钙离子有交换能力,理论交换能力为352CaCO3mg/g,一般为290~320mgCaCO3/g,白度≥95%,pH值10~11.5,表观密度0.3~0.5g/cm3,平均粒径为2μm,粒度分布≤4μm占85%以上。用作无磷洗涤剂的助剂,代替三聚磷酸钠;在石油和其他工业用作气体和液体的干燥、脱水净化等,也用作催化剂和软水剂。