1) Sidepiece Rebuilds

侧部重造
1.
The breakage in sidepiece inner liner is repaired by using " Sidepiece Rebuilds" method, the plant practice shows that it is feasible on technique and reasonable on economic.
某公司3台200kA级大型预焙槽侧部内衬早期破损的主要原因是:铝电解槽热损失分布不合理,局部熔体冲刷严重,采取“侧部重造”补救办法对侧部内衬破损处进行修补。
2) re-making of side carbon block

侧部碳块重塑法
1.
The paper describes the re-making of side carbon block - a method for repairing incipiently damaged side of the large pre-baked aluminum smelting cell, which allows no stop of cell, smooth operation of cell after minor repair and a cell life extension of 345 day on average.
介绍了大型预焙铝电解槽侧部早期破损的修补方法——侧部碳块重塑法,此方法不需要停槽操作,经小修后的电解槽运行平稳,槽寿命平均延长345d。