说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 丝状锈
1)  filamentous rust
丝状锈
1.
This paper puts forward the method for preventing the fil-amentous rust, which results in no significant variation in the film appearance, adhesion and mechanic strength etc; the filamentous rust develops slowly and there is no deep corrosion at the steel layer, no evident influence on the protection and usability of the elec.
提出了克服丝状锈的措施。
2)  filiform [英]['filifɔ:m]  [美]['fɪlə,fɔrm]
丝状锈蚀
3)  stainless steel wire
不锈钢丝
1.
Technology of removing deformation magnetic property of metastable austenite stainless steel wire
消除亚稳定奥氏体不锈钢丝形变磁性的技术
2.
The microstructure and mechanical properties of stainless steel wires used for metal rubber were studied by means of optical microscopy,SEM,and X-ray diffraction.
15mm的Cr-N i-Mn系不锈钢丝的微组织结构和力学性能的变化规律。
3.
There is a coat of oxide on the surface of the heat treated stainless steel wire,which is difficult to be cleaned.
不锈钢丝热处理后表面形成一层难以清除的氧化皮 ,4 80℃高温碱煮和 85℃高锰酸钾碱液的清洗对比试验和应用显示高锰酸钾碱洗工艺可行 ,但要求KMnO4 和NaOH浓度大于 80g L ,溶液温度高于 80℃ ,清洗时间5~ 10min ,比碱煮少 5min ;高锰酸钾碱液清洗效果好 ,不锈钢丝表面无黑色胶状物 ,而且不会产生过腐蚀 ,每吨不锈钢丝可节省电能 1875kW·h ,劳动环境也有很大改
4)  steel wire anticorrosion
钢丝防锈
5)  rustysilk
锈渍纬丝
6)  steel wire corrosion
钢丝锈蚀
补充资料:丝状锈蚀
分子式:
CAS号:

性质: 由于漆膜下面的金属表面发生了细丝状的腐蚀,导致漆膜表面出现疏松的线状隆起。这种线状腐蚀常由一个或几个腐蚀生长点辐射而成。对于钢铁底材,这种病态也称丝状锈蚀,俗称“红丝”。温度在21~35℃、相对湿度60%~95%时,最容易发生这类腐蚀。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条