1.
The method of sintering Ni-Mo ores under 600 ℃ to remove sulfur,and then lixiviating under the alkaline and active-oxygen condition was advanced to solve the problem of extracting molybdenum from the rocky-select Nickel-Molybdenum ores in this paper.
文章针对从难选镍钼矿中提取钼的问题,提出了一种先将镍钼矿在600℃时焙烧脱硫,再将其加碱和通活性氧气浸出的方法,并通过对比试验确定了最佳的工艺条件:氢氧化钠30%(或碳酸钠50%),浸出液固比为3∶1,温度90~100℃,反应时间3 h。