说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
|
|
|
您的位置: 首页 -> 词典 -> 双向拉伸聚对苯二甲酸乙二酯
1) BOPET
双向拉伸聚对苯二甲酸乙二酯
1.
The production technology of BOPET film including PET drying,extrusion casting,biaxial tension,coiling and deep-processing was presented in detail.
详细介绍双向拉伸聚对苯二甲酸乙二酯(BOPET)薄膜的生产工艺,包括PET树脂干燥、挤出铸片、双向拉伸、卷取和深加工,并对经常出现的疵病如不熔物、厚度不均、条道、疵点、气泡、穿孔、划痕等进行分析,给出了相应的解决方法。
2) tensilized poly films physprop
拉伸聚对苯二甲酸二乙 薄膜
3) PET
[英][pet] [美][pɛt]
聚对苯二甲酸乙二酯
1.
Study on the Preparation, Structure and Properties of PET/Montmorillonite Based Nanocomposites;
聚对苯二甲酸乙二酯/蒙脱土纳米复合材料的制备及结构性能研究
2.
PET/nano BaSO4composites were manufactured by melt blending process.
通过熔融共混法制备聚对苯二甲酸乙二酯(PET)/纳米BaSO4复合材料,研究了纳米BaSO4对PET结晶行为、力学性能及热性能的影响。
3.
The research development of poly(ethylene terephthalate)(PET)blended with polypropylene (PP)was reviewed.
综述了聚对苯二甲酸乙二酯(PET)和聚丙烯(PP)共混的研究进展。
4) Poly(ethylene terephthalate)
聚对苯二甲酸乙二醇酯
1.
Poly(ethylene terephthalate)(PET)and PA5935 were blended in a high speed mixer,and then injected into specimense.
将聚对苯二甲酸乙二醇酯(PET)与PA5935高速共混,注射制样,样品的热性能、力学性能、阻燃性能和流变性能等测试结果表明,在PET中加入少量PA5935改善了PET抗熔滴性能与炭化性能,但结晶度、氧指数和部分力学性能下降。
2.
The immiscible poly(ethylene terephthalate)(PET)/polypropylene(PP)blend was prepared by melt mixing and its structural rheology was studied.
通过熔融共混制备了不相容的聚对苯二甲酸乙二醇酯(PET)/聚丙烯(PP)复合体系,研究了复合体系的结构流变学。
3.
The feasibility of in-situ microfibrillar method on recycling poly(ethylene terephthalate)(PET) and high-density polyethylene(HDPE) mixtures was carried out by four repetitive extrusion.
研究了原位微纤化方法在回收聚对苯二甲酸乙二醇酯(PET)和高密度聚乙烯(HDPE)混合物方面的应用。
5) poly(ethylene terephthalate)
聚对苯二甲酸乙二酯
1.
Research on non-isothermal crystallization kinetics of poly(ethylene terephthalate);
聚对苯二甲酸乙二酯非等温结晶过程研究
2.
The non-isothermal degradation processes of poly(ethylene terephthalate)(PET) and poly(ethylene 2,6-naphthalate)(PEN) blends were studied by using thermogravimetry(TG) analysis in nitrogen.
研究了惰性气氛下聚对苯二甲酸乙二酯(PET)/聚对萘二甲酸乙二酯(PEN)共混物的非等温热分解行为及其动力学。
3.
The poly(ethylene terephthalate) /montmorillonite nanocomposites are prepared by melt intercalation process and the crystallization behaviors, mechanical properties and dyeing properties of the fibers are studied in detail .
采用熔融插层法制备聚对苯二甲酸乙二酯(PET)/蒙脱土(MMT)纳米复合材料,对其纤维的结晶性能、力学性能及染色性能进行详细研究。
6) PET
[英][pet] [美][pɛt]
聚对苯二甲酸乙二醇酯
1.
Interaction Parameters of the PET/PC and PET/Phenoxy Resin Blends;
聚对苯二甲酸乙二醇酯与聚碳酸酯及聚酚氧树脂间的相互作用参数
2.
Preparation of PET/MWNTs Nano Composite by Covalent Grafting;
多壁碳纳米管与聚对苯二甲酸乙二醇酯的接枝聚合
3.
The grafting product was used as the reactive compatibilizer of HDPE/PET blend and the influences of the compatibilizer on mechanical properties, thermostimulative shape memory function of blends were discussed.
结果表明:采用GMA/St双组分单体具有较高的接枝率,生成的接枝物对HDPE/聚对苯二甲酸乙二醇酯(PET)共混合金的增容效果较好;提高了体系的力学性能和热致形状记忆性能,且HDPE-g-(GMA-co-St)含量为5~10phr时,合金具有较好的综合性能。
补充资料:拉伸模的常有缺陷二
凸模肩部相应部位裂纹 由于材料的强度不够,当拉深载荷达到材料破断载荷时就会发生此缺陷。 缺陷部位产生于凸模肩R相应的部位(rp处),即比冲撞痕线更接近rp的部分。破裂部分的冲撞痕线,因与其他部位不同,可以对下面几种情况进行观察检查:或者被延展;或者在凸缘的上下面有发亮的部分;或者产生折皱。另外,在侧壁上有时也有发亮的部分。 初期横向破裂,呈舌状。 原因及消除方法 (1)制品形状。 ① 拉深深度过大。 目前,圆筒、方筒深拉深的极限是在设计阶段确定的。从而,在极限附近进行拉深时,要用表面光洁、平整的材料,综合模具配合和研磨,加工润滑油,缓冲压力,压力机精度等现场条件,进行试验拉深。 ② 凸模半径(rp)过小。 a 将rp修正到适当值。 b 图纸上的rp过小时,首先按适当值进行拉深,然后再增加一道工序,成形所需尺寸。 ③ 凹模尺寸(rd)过小。 a 将rd修正到适当值。 b 图纸上的rd过小时,首先用适当rd值进行拉深,然后再增加一道工序,成形到所需尺寸。 ④ 方筒的角部半径(rc)过小。 a 将拉深深度减小; b 多增加一道拉深工序; c 换成更高级的材料; d 将板料厚度增加。 (2)冲压条件。 ① 压边力过大。 压边力过大时,在凸缘面上不会发生起皱。防皱压板面粗糙度,模具配合,间隙,rp,rd,加工油的种类和涂敷条件,缓冲销造成的压边力分布等,都影响防皱压力。如果有关拉深的上述这些条件都合适的话,压边力就会下降,在起皱之前,不会发生破裂。 压边力过大时,由于凸缘面会全面发亮,所以很容易判断。 ② 润滑不良。 拉深加工与润滑有极为密切的关系,特别是包含有减薄拉深加工时,必须控制制品温度的升高。如果是条件好的拉深加工,润滑油的选择不成什么问题;条件不好的拉深加工,如果润滑油选择不当,就会引起破裂。 ③ 毛坯形状不良。 在试拉深阶段,决定毛坯形状是重要的工作之一。 必须将毛坯形状限制在最小尺寸。当用方形毛坯进行圆筒拉深时,极限拉深率为0.58左右。另外,如果拉深率过于严苛,rp部位的伤痕会产生破裂,如进行切角,就可防止破裂。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条
|