说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 高温压缩永久变形试验
1)  compression set test at high temperature
高温压缩永久变形试验
2)  thermo compression set
高温压缩永久变形
1.
In this paper,the influence of the ratio of the CR/PUR blends on the curing characteristic,mechanical property,hot ageing resistance and thermo compression set of the blends were studied.
研究了共混比对氯丁橡胶/聚氨酯橡胶(CR/PUR)的硫化特性,硫化胶力学性能、耐热老化性能以及高温压缩永久变形的影响。
3)  compression set
压缩永久变形
1.
Study on compression set of EPDM vulcanizates
EPDM的压缩永久变形性能研究
2.
Properties of stress relaxation and compression set of vulcanite during isothermal thermo-oxidative aging
硫化胶等温热氧老化时应力松弛和压缩永久变形性能的研究
3.
The effect of blend ratioes on the mechanical properties,ageing resistance properties,oil resistance porperties,compression set and dynamic mechanical properties of PUR/CR,CSM/NBR,EPDM/IIR blends were also researched.
研究了PUR/CR,CSM/NBR,EPDM/IIR几种合成橡胶的共混和硫化特性,以及共混比对共混胶力学性能、耐热老化性能、耐油性能、压缩永久变形和动态力学性能的影响。
4)  compression set
压缩永久形变
1.
Compression Set of SEBS/PP Elastomer Modified with PPO;
PPO改性SEBS/PP共混体系压缩永久形变的研究
5)  The permanent compression set value
压缩永久变形率
6)  high temperature compress test
高温压缩试验
补充资料:高温压缩永久变形试验
分子式:
CAS号:

性质:考察橡胶制品在高温压缩状态下永久变形的试验。测定时将试样进行一定压缩后,放在高温下保持一段时间,然后在室温下冷却2h,除去负荷后再自由恢复1h,最后测定试样高度,高温下压缩永久变形率K由下式计算。式中,h0、h1、h2分别为压缩前压缩下和恢复后的试样高度。