2) Tussah Silk Fabric Aftertreatment finishing agent

柞蚕丝织物整理剂
3) tussah cloth

柞丝绸
1.
Tussah cloth was creaseproofing finished with water-solubility epoxide as formaldehydeless finishing agent.
对不同工艺条件下几个重要的影响整理因素进行分析讨论,获得无甲醛整理剂——HY-001对柞丝绸防皱整理的优化工艺。
4) Tussah silk

柞丝绸
1.
A theoretical formula about the relationship of the thickness and crease recovery angle of tussah silk was established.
对柞丝绸的厚度及折痕回复角进行了测试,并且通过SPSS统计分析软件对柞丝绸的厚度与折痕回复角的相关性作了回归分析,分析发现,该织物厚度与折痕回复角的相关程度较大,并从理论上建立了柞丝绸的厚度与折痕回复角的函数关系式。
2.
Polycarboxylic acid-the copolymer(PMA) of maleic acid(MA) and itaconic acid(IA) was synthesized and applied to tussah silk for crease-proofing finish.
合成马来酸(MA)、依康酸(IA)共聚物(PMI),用于柞丝绸的抗皱整理,通过正交试验优选了其在柞丝绸防皱整理中的应用工艺,结果表明:织物经PMI整理后,湿弹性显著提高,耐洗性较好,对织物的白度和强度基本无影
3.
Acid or neutral dyes low_temperature dyeing experiment of tussah silk is conducted in buffer solution acetic acid in the presence of sodium acetate,penetrant and dye leveller in order to obtain optimal dyeing conditions.
采用缓冲溶液醋酸—醋酸钠和添加渗透剂、匀染剂,对柞丝织物酸性染料和中性染料低温染色工艺进行试验,得到柞丝绸低温染色的最佳工艺条件。
5) tussah silk

柞蚕丝绸
1.
The application of natural dyestuff-Coptis Chinensis on dyeing of the tussah silk was discussed,and the optimal process was given.
探讨了天然染料黄连在柞蚕丝绸染色中的应用,确定出合理的染色工艺。
2.
As treasured gem, silk is highly regarded as an indispensable part of voluminous Chinese cultures, and tussah silk in particular holds its exclusive position for its crude plainness.
天然雕饰的柞蚕丝绸产品更是丝中珍品,有其不可取代的独有品性。
6) tussah noil yarn

柞蚕绸丝
补充资料:变形丝织物
用变形纤维织成的织物,包括高弹和低弹织物。化学纤维长丝经过一次加热变形制成的螺旋圈形,弹性伸缩率较高,称高弹丝,制成的产品称高弹织物。如锦纶或丙纶弹力衫裤、弹力袜、弹力游泳衣等。高弹丝再经一次热松弛定形,则呈膨松卷曲状,弹性和伸缩率较低,称为低弹丝,可织成低弹织物,如各种涤纶变形丝织制的仿毛、仿丝、仿麻型的针织物和机织物(见彩图)。变形纤维在纺织染整加工过程中,须严格控制拈度、张力、温度和加热时间等工艺条件,尽量减少对织物弹性和膨松性的影响。另外,如采用5~10叶异形截面纤维可以增加织物的弹性;采用细于1旦的化纤丝可以改进织物的柔软性和覆盖丰满性;采用不同卷曲形态、不同拈度、不同纤度的混纤变形丝,可以增加织物的真丝感或毛感。