2) ultra-low sulfur steel

超低硫钢
1.
Investigation on slag modifier during refining of ultra-low sulfur steel;

超低硫钢冶炼过程钢包渣改质剂的作用
2.
The theoretical analysis and commercial experiment of desulfuration of ladle furnace for the refining of ultra-low sulfur steels are carried out in this paper,the results are: optimizing the composition of slag,increasing the optical basicity,deeply deoxidizing of both molten steel and slag;determining the proper slag weight are the effective methods of increasing the sulfur removal percentage.
对超低硫钢生产过程中LF精炼渣脱硫进行了理论分析与工业试验,结果表明:优化精炼渣成分,提高光学碱度,强化钢水及炉渣脱氧,选择合适的渣量是提高脱硫效率的有效手段;武钢管线钢生产中LF平均脱硫率为55%;CaO-SiO2-Al2O3-MgO(5%)渣系等硫分配比曲线图可指导生产选择合适的炉渣成分。
3.
On the base of theoretic analyzing, the ladle slag modification treating test were done during the melting of ultra-low sulfur steel.
本文在理论分析的基础上,在超低硫钢冶炼过程中对转炉出钢下渣进行了改质处理试验。
3) Ultra-Low Sulphur Steel

超低硫钢
1.
Process for Production of Ultra-Low Sulphur Steel by BOF Tapping Desulphurizing-LF Refining;
氧气转炉出钢脱硫-LF精炼生产超低硫钢的工艺
2.
High Sulphur Capacity Slag Series Containing BaO for Ultra-Low Sulphur Steel Refining;

高硫容量含BaO超低硫钢精炼脱硫渣系
3.
Smelting Technology of Refining Ultra-Low Sulphur Steel by RH Process;

RH工艺精炼超低硫钢的冶炼技术
4) ultra low sulfur steel

超低硫钢
1.
A thermodynamic calculation method was used to determine the process parameters of ladle furnace for the refining of ultra low sulfur steels.
提出了采用热力学计算分析确定LF炉冶炼超低硫钢工艺条件的方法·分析表明 ,可通过提高炉渣碱度、强化渣钢脱氧、控制渣钢原始硫质量分数和渣质量 ,来实现超低硫钢的冶炼·15 0tLF炉生产实践表明 ,在原始钢水硫平均为 0 0 14 6%条件下 ,通过控制规定的工艺条件 ,经LF处理后的钢水硫质量分数平均可达 0 0 0 44 % ·再经VD处理后 ,可实现成品硫质量分数为0 0 0 2 7%的超低硫钢生产·在上述条件基础上 ,将原始硫质量分数控制在 0 0 0 5 8%以下或保证渣金硫的分配比在 2 5 0以上或采用双渣操作 ,LF炉可精炼 0 0 0 2 %以下极低硫
5) ultra-low carbon and sulphur

超低碳硫
6) ultra-low sulfur diesel

超低硫柴油
1.
The technical measures include facing the trends of crude oil more inferior and heavier;supply of ultra-low sulfur diesel and clean gasoline;and increasing the economic effect and reducing the pollutant exhaustion.
介绍了2006年NPRA年会报道的炼油工业适应原油变化和确保产品供应的技术措施,主要包括应对原油资源劣质化和重质化的技术措施,应对超低硫柴油供应的技术措施,应对清洁汽油供应的技术措施以及提高催化裂化效益和降低其污染物排放的技术措施等。
2.
The performances of new hydrogenation catalyst of KF760,KF767 and the hydrocracking pretreat catalysts of KF860 developed by Albemarle Corporation,United States,were introduced,which were used to produce ultra-low sulfur diesel.
介绍了美国Albemarle公司开发的用于生产超低硫柴油的新型加氢催化剂KF760、KF767以及加氢裂化预处理催化剂KF860的性能:指出加氢处理技术是生产清洁燃料的重要手段之一,未来的炼油工业将呈现原油加氢处理能力快速增长的趋势。
3.
Based on the physicochemical properties of the fractions of low sulfur and ultra-low sulfur diesel fuels from hydro-refining,hydrogen under medium pressure and hydro-cracking,the relationship(between) lubricity and properties of diesel fuels was analyzed.
在分析加氢精制、中压加氢改质和高压加氢裂化生产的低硫和超低硫柴油馏分理化性质的基础上,探讨了柴油的理化性质与润滑性能的关系;采用逐步线性回归的方法,建立了每克柴油中硫少于200μg的加氢柴油润滑性能预测模型,预测值与实测值的相对误差在7%以内。
补充资料:超低界面张力
分子式:
CAS号:
性质:关于油水体系界面张力,一般把10-1到10-3mN/m算作低界面张力,将10-3mN/m以下的称超低界面张力。超低界面张力在第三次采油中具有重要意义。研究表明,在注水驱油中,如果使界面张力降低三个数量级,就可以使地层残油体积减少一半,若能使界面张力降低四个数量级,理论的驱油率可达100%。
CAS号:
性质:关于油水体系界面张力,一般把10-1到10-3mN/m算作低界面张力,将10-3mN/m以下的称超低界面张力。超低界面张力在第三次采油中具有重要意义。研究表明,在注水驱油中,如果使界面张力降低三个数量级,就可以使地层残油体积减少一半,若能使界面张力降低四个数量级,理论的驱油率可达100%。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条