1) polarization fatigue

极化疲劳
1.
However,its application in ferroelectric random access memories(FeRAMs) has been hindered due to serious polarization fatigue upon repeated domain switching,so that it has eventually been replaced by layered perovskite ferroelectric Sr2BiTa5O9(SBT),among others.
然而,在将它应用于铁电存储时,PZT薄膜遭遇到极化疲劳问题而被SrBi2Ta2O9(SBT)等铁电体所替代,这一问题至今未能得到妥善解决。
2.
In this paper we report the studies on polarization fatigue in ferroelectric vinylidene fluoride and trifluoroethylene copolymer films.
本文研究了有机铁电薄膜的极化疲劳过程。
3.
Based on the oxygen vacancies electro-migration to interfacial layer, generation of new vacancies due to deoxidization of high valence cations by injected charges and local phase decomposition(LPD) a physical image of polarization fatigue is derived.
铁电薄膜的极化疲劳是导致存储单元失效的最重要的因素之一,人们进行了大量的研究来探寻极化疲劳的机理,然而至今仍没有一个令人满意的物理模型。
2) fatigue limit

疲劳极限
1.
Influence of surface integrality on fatigue limit for 30CrMnSiNi2A steel;

表面完整性对30CrMnSiNi2A钢疲劳极限的影响
2.
Quantitative study on influence of chemical heat treatment on apparent fatigue limit of 40Cr steel;
化学热处理对40Cr钢表象疲劳极限影响的定量化研究
3.
Acquisition system unit about the infrared image of fatigue limit of metal based on USB2.0;
金属疲劳极限快速检测的USB2.0数据采集单元设计
4) fatigue point

疲劳点;疲劳极限
5) intensifying fatigue

疲劳强化
1.
The intensifying fatigue of rubber/polyester cord composite depended mainly on the nature of composite materials.
聚酯 /橡胶复合材料的疲劳强化现象主要与组分材料本身的特性有
6) fatigue hardning

疲劳硬化
补充资料:ADS疲劳试验
分子式:
CAS号:
性质:考察橡胶裂口增长的一种疲劳试验方法,该法由E. E. Auer、K. W. Doak和I. J. Schaffiner三人首先提出,也由此而得名。试验利用德墨西亚疲劳试验机测定初始割口直径Φ0.93mm在屈挠频率为287次/min下,割口增长和300%定伸应力变化情况。
CAS号:
性质:考察橡胶裂口增长的一种疲劳试验方法,该法由E. E. Auer、K. W. Doak和I. J. Schaffiner三人首先提出,也由此而得名。试验利用德墨西亚疲劳试验机测定初始割口直径Φ0.93mm在屈挠频率为287次/min下,割口增长和300%定伸应力变化情况。